Abstract
In this study, the influence of the wettability on antifouling performance of glass-ceramic coatings (GCCs) was investigated. Two coating systems—alkali-silicate (AS-GCC) and alkali-borosilicate (ABS-GCC)—with SiO2/B2O3 molar fractions of 9.49 and 2.87, respectively, were designed to achieve distinct surface wettability. Comprehensive characterization was conducted using X-ray fluorescence (XRF), (differential thermal analysis) spectroscopy, thermogravimetric-differential thermal analysis (TG–DTA), Fourier Transform Infrared (FTIR), X-ray diffraction (XRD), Scanning Electron Microscopy/ Energy Dispersive X-ray (SEM/EDX), Contact Angle (CA) measurements, and three-dimensional non-contact optical profilometry (NCOP). Antifouling performance was evaluated under natural seawater exposure conditions. The AS-GCC exhibited a higher contact angle (63.0°), whereas the ABS-GCC showed a more hydrophilic surface (27.7°). A lower contact angle was associated with a lower barnacle settlement density, with ABS-GCC showing 68.9 barnacles/cm2 compared to 88.7 barnacles/cm2 for AS-GCC. Post-test surface analyses confirmed complete foulant removal without coating damage, while NCOP revealed only minor roughness changes, indicating resistance to microbially induced corrosion (MIC). These results demonstrate that glass-ceramic coatings are durable and environmentally benign antifouling materials for seawater applications, and that tailoring the SiO2/B2O3 molar ratio provides an effective approach to tuning surface wettability and antifouling performance.
Keywords
Subject Areas
OpenAlex SDG Match
SDGs auto-classified by OpenAlex (score ≥ 0.4 shown).